PowerResins Vintage Castable Resin
186,00€ ME ΦΠΑ
PowerResins Vintage Resin
Developed for directly casting jewelry with great details. Perfect for producing chain models and gourmet series.
-
Especially suitable for chain models.
-
Perfect printing properties with sharp details suitable for jewelry with micro-pave prongs, engraving, highly detailed figures or filigree.
-
Easy to set stones directly on printed model before casting.
-
Create lighter jewelry with perfect precision.
-
Perfect 100% ash-free burnout for direct casting.
-
Use of standard wax burnout cycle.
-
No need for post-curing after printing
Έρχεται σε μπουκάλι των 500ml. Άμεσα διαθέσιμη!
VINTAGE resin offers a versatile one-stop solution for all types of jewelry manufacturing needs, offering superb direct casting results with an unseen non-shrinking formula allowing you an easy ash-free resin casting process like a traditional lost wax casting . With VINTAGE resin, compromise is a thing of the past; enjoy smoother surfaces and razor-sharp edges in every print. Additionally, it’s perfectly tailored for intricate stone settings, ensuring precision and quality in every piece.
- Shrinkage rate is less than %1
- Ash-free casting like a wax
- No need post curing
- Perfect for stone settings
- Find here printing parameters for DLP and LCD printers
Casting and Burnout Cycle for PowerResins Castable Resins
1. Washing the Models
- 3 minutes with clean alcohol (that is minimum 90% pureness).
- Wash 2 minutes with dirty alcohol then dry by blowing air (an air compressor can be used) and then 2 minutes with clean alcohol then dry by blowing air.
- Check the models, if there are uncured resin on the model wash and dry them again.
- The models should not be exposed to alcohol for more than 6 minutes.
- First choice for alcohol; ethyl alcohol is suggested. Otherwise; isopropyl alcohol can be used.
- Models should be casted as soon as possible (within 2 hours is suggested). The models must always be stored in a dark and ideally in a sealed plastic bag.
2. Investment Process
- Instructions (water-powder ratio, mixing process etc.) by the manufacturer of the investment must be followed.
- Must be make sure that the investment gets vacuum very well. The vacuum process must be aplied by vibrating the investment.
- Casting tree should be inserted as far away from the surface of the flask as possible (! Do not put the printed model close to the flask’s wall).
Note: Every steps should be completed by the professional machines. Every detail is essential to get applied correctly.
3. Recommended Burnout Cycle
- Before insterting the flask into furnace, flask must be left settled for minimum 3 hours.
- In the last step of the cycle; after ramp down to 600 Celsius degrees within 1 hour, the flask should stay in the furnace at 600 Celsius degrees for about 1 hour before pouring the metal.
- Fresh metal should be used to cast. Metals used for many times (more than 3-4) to get casted should not be used.